How Copper Dissolution Affects ALS2 Gold Yield in Mixed PCB Scrap

Mixed printed circuit boards contain copper in tracks, connectors, pads, shielding and plated through-holes. The effect of copper dissolution on ALS2 gold yield in mixed PCB scrap is rarely a simple loss. Copper can expose gold-bearing surfaces while also increasing chemical demand, changing downstream separation conditions or diluting the gold-bearing product.

For Australian operators, this interaction must be considered alongside local collection habits, waste legislation, transport distances and the economics of recovering gold from lower-grade mixed boards. ALS2’s acidless separation approach reduces reliance on conventional mineral-acid refining, but copper remains a central variable in determining consistent, commercially meaningful recovery.

Copper behaviour starts with feed heterogeneity

Mixed PCB scrap is not a uniform raw material. Boards from office computers, mobile phones, industrial controls and household appliances contain different copper-to-gold ratios, laminates, solder compositions and shielding materials. A connector-rich fraction may dissolve readily, while gold trapped beneath solder, epoxy or other coatings may require different liberation conditions.

The resulting gold yield depends on how much copper enters the reaction phase, how rapidly it dissolves and where it goes afterwards. Copper dissolution can increase the available surface area of some gold-bearing components, potentially improving access. However, higher dissolved-metal loading can also narrow the operating window in which gold separates selectively.

Acidless does not mean chemistry-free. ALS2 still relies on controlled chemical and physical conditions to distinguish valuable metals from the wider PCB matrix. Copper therefore has to be treated as an active process variable rather than background contamination.

How dissolution changes ALS2 separation

When copper dissolves, it can consume part of the available oxidising or ligand-forming capacity. A change in redox conditions may alter how readily gold, palladium and other target metals dissolve or remain associated with solid residues. The effect is especially relevant when the feed contains much more copper than the process was calibrated to handle.

Copper can also influence physical separation. Fine copper-rich particles may coat gold-bearing surfaces, increase residue filtration pressure or carry valuable metals out with the discarded solid phase. Conversely, selective copper removal may open pathways that were previously blocked. The outcome depends on feed preparation, particle size, reagent conditions and solid-liquid separation.

Further context on selective dissolution and recovery kinetics is available in the selective separation notes. These principles help explain why copper dissolution should be tracked throughout the ALS2 flowsheet rather than assessed only through the final gold result.

Australian feed streams add practical variability

Sydney, Melbourne, Brisbane and Perth generate substantial electronic waste through household upgrades, office refurbishments and commercial equipment replacement. Computers, phones, printers and networking equipment often pass through different collection routes before reaching a recycler, making the final PCB mixture less consistent than a dedicated industrial stream.

Many Australian households place old electronics in storage or general waste because they are unsure how to recycle them. Council e-waste days, approved collection services and retailer take-back programs are improving, but their coverage varies between municipalities. NSW’s Waste Avoidance and Resource Recovery Act, Victoria’s Environment Protection Act and similar state regimes make responsible handling and traceability essential.

Australia’s National Waste Policy aims to reduce waste sent to landfill by half by 2030, creating a favourable policy direction for high-recovery recycling. Local gold refining, bullion production and the country’s ASX-listed mining sector also provide established markets, although recovered material must be evaluated against gold prices denominated in Australian dollars and the cost of moving low-value scrap over long distances.

Feed or process condition Copper-linked change Likely effect on gold measurement Control or verification
Connector-rich boards More copper available to dissolve, with greater reagent demand Gold may be exposed while separation selectivity falls Assay copper by board fraction and establish a copper-specific dose response
Fine PCB dust High surface area and mixed-metal loading Fast dissolution can be confused with solids carryover Control solids concentration and include wash-down recovery
Copper-rich residue Copper remains with unliberated gold Reduced recovered gold despite reasonable chemical dissolution Improve phase separation and chemically test the residue
Copper reporting to product Product mass increases without proportional gold Lower gold tenor rather than necessarily lower gold recovery Report recovered grams separately from product mass
Changing operating conditions Redox or ligand conditions drift between batches Inconsistent dissolution and gold yield Record operating conditions and analyse duplicate feed splits

Measuring gold yield with a closed mass balance

Gold yield can mean recovered grams per tonne, percentage recovery from the feed or the gold tenor of a concentrate. Those measures are not interchangeable. If copper enters a gold-bearing product, its mass may increase while the percentage of gold in that product falls. Absolute recovered gold can remain unchanged, so the result must not be described as a loss of extraction.

A reliable assessment begins with representative sampling of the original mixed PCB scrap. Gold and copper should be assayed across the incoming fraction, reacted solids, wash solutions and final product. Solids left in equipment, filters and piping also need to be included, because retained residue can conceal otherwise successful dissolution.

Feed and product measurements should be supported by duplicate tests at several copper levels. Testing a low-copper fraction alone may create a misleading benchmark, while a single high-copper batch cannot establish a process relationship. The useful result is a copper-response curve supported by reagent consumption, residue composition, solution metal loading and independently measured gold recovery.

Safety and economics of compact recovery

The acidless ALS2 concept offers a route to safer separation by avoiding the handling of large volumes of corrosive mineral acids. It does not remove the need for industrial controls. PCB shredding can create dust containing lead and other hazardous constituents, while brominated flame retardants, residual process reagents and metal-rich residues require appropriate classification and management.

Compact plants can reduce transport costs when located near established urban e-waste aggregation points. Their viability depends on more than the spot gold price. Sorting, preprocessing, chemical consumption, labour, energy, residue treatment and the saleability of copper-rich by-products all affect the operating margin. A plant that maximises gold recovery but produces excessive contaminated residue may be less bankable than one with balanced metal recovery.

ALS2Project’s support from the European Union’s Horizon 2020 research and innovation programme offers a basis for technical due diligence. Australian deployment still requires validation with local feed chemistry, local regulations and realistic logistics. Equipment scale should follow those findings rather than a laboratory result based on unusually rich or homogeneous scrap.

Building an Australian ALS2 recovery pathway

The first practical step is to create a characterised feed source rather than buying an ungraded pile of circuit boards. Separate boards by source where possible, remove bulky metal components and sample each fraction for gold, copper and other relevant metals. This reveals whether dilution is reducing the observed ALS2 gold yield or whether copper dissolution is actively impairing separation.

A controlled trial should then compare representative mixed PCB scrap with a defined copper-response series. Each batch needs full gold and copper balances across feed, product and residue, together with records of reagent use and operating conditions. Where results are promising, the next stage should evaluate safe residue routes, electricity and reagent supply, transport requirements and compliance with the relevant state waste regulations.

To move the ALS2 technology beyond laboratory performance, Australian recyclers, refiners, e-waste collectors and research partners should cooperate on representative sampling and independent mass balances. Commission a copper-controlled ALS2 trial on Australian PCB scrap, with gold recovery and residue safety reported together, and publish the operating envelope needed for a safe, bankable recovery plant.